A 1,500 V DC photovoltaic (PV) string can remain on a roof, carport or tracker for 25 years. The connector is inspected; the cable jacket is often not. The outer sheath takes the...
A 1,500 V DC photovoltaic (PV) string can remain on a roof, carport or tracker for 25 years. The connector is inspected; the cable jacket is often not. The outer sheath takes the...
Compound Evaluation Guide A 105 °C PVC automotive wire compound can pass a 240-hour oven test and still crack inside a transmission tunnel after 3,000 hours at the same nominal te...
A compound that passes every incoming inspection can still fail on your extruder. The usual cause is not a bad batch. It is a specification that described the pellet instead of t...
A 33 kV feeder laid in saturated clay and a submarine export cable crossing a tidal landfall fail for the same reason: water reaches the insulation screen. In both cases the deci...
A Medical Polyvinyl Chloride Compound is not defined by its base resin alone — flexibility, transparency, chemical resistance, and processing behavior all come from the combinatio...
A 90 °C halogen-free sheathing compound can pass the single-wire EN 60332-1-2 flame test and still fail the Cca classification written into the purchase order. EN 50399 measures ...
When a 132 kV cable fails its routine partial-discharge screen at 5 pC, the extrusion line is examined first and the compound is examined last. The order is usually reversed. Par...
Three hours into the first run of a low-smoke halogen-free sheath compound, the operator at a cable plant in Hangzhou watched the extruded surface turn chalky, a white ring form o...
Every metre of cable under a metro carriage floor is a potential fuel source, and inside a tunnel fire the real hazard is usually not the flame itself. Smoke, hydrogen chloride, a...
Every cable manufacturer has heard a variation of the same warning: a batch of low-smoke halogen-free (LSZH) compound extrudes cleanly, produces a smooth cable surface, and passes...
Two cable factories receive quotations for the same thermoplastic low smoke zero halogen (LSZH) sheath grade. One supplier quotes 15 percent lower, and its datasheet looks nearly ...
A cable producer qualified an LSZH jacket compound for a rail project and watched the extrusion surface turn rough within the first hour of production. Another buyer saw the same ...